This study investigated the drying of spiral and flotation coal filter cakes using activated alumina as an adsorbent. The experiments were done on a laboratory-scale rotating bed with the coal being dried in a cascading motion inside cylindrical vessels. The adsorbent-to-coal mass ratio, adsorbent particle size and adsorbent state (new, used or regenerated) were varied to study each variable’s effect on the drying performance. The coal’s heating values were measured at significant intervals during drying to do an energy balance on the process, determining the feasibility thereof from an economical and energy perspective. The study found that the spiral and flotation coal fines could be dried swiftly to a market specified moisture content of 10% w/w within two minutes’ contact sorption.
Related Products
Guideline for Mine Closure Relinquishment Criteria
2023
Review of closure and relinquishment law in Australia, Canada and South Africa, with four mechanisms for reaching agreement compared. For closure planners and regulators.
What this report foundRelinquishment criteria follow from the agreed post-mining land use. The land use is the goal and the criteria measure whether it has been reached.
R1500,00
Relinquishment criteria follow from the agreed post-mining land use. The land use is the goal and the criteria measure whether it has been reached. The guideline sets out a framework for approving those criteria at each mining phase, from the initial environmental management plan through to decommissioning, and compares South African practice with Australian, Canadian and international guidance.
Flammability, corrosion resistance and environment by V Mhlawakhe.pdf
Laboratory work turning high ash coal fines into moulded building composites, comparing coal tar pitch against a silicone binder, with strength, burning, corrosion and leaching tests. For product developers.
What this report foundAir blowing converted coal tar into a pitch with 11.27% volatile matter and 87.68% fixed carbon, which bound high ash coal fines into structural composites.
R1500,00
Air blowing converted coal tar into a pitch with 11.27% volatile matter and 87.68% fixed carbon, which bound high ash coal fines into structural composites. Compressive strengths ran from 106.58 to 344.71 MPa and flexural strengths from 48.75 to 159.30 MPa. Flammability was low across all composites and corrosion rates stayed below those of some commercial ceramic tiles.